300M (low carbon quenched tempered is 300M low alloy steel (UNS K44220, EN 41SiNiCrMoV7-6) in the (low carbon, quenched & tempered condition. This 300M (low carbon quenched tempered material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all 300M conditions in our 300M yield, tensile and hardness comparison . Looking for 300M parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined 300M steel parts in-house and inspects them before shipment.
300M (Low Carbon, Quenched & Tempered Designation
0.40C 300M Condition Quenched & tempered UNS number K44220 US name AMS 6417, 4340M, MIL-S-8844 EN name BS S 155, 41SiNiCrMoV7-6 EN number 1.6928
300M (Low Carbon, Quenched & Tempered Typical uses
General construction, general mechanical engineering, automotive, pressure vessels, pipework
300M (Low Carbon, Quenched & Tempered Composition detail
C (carbon) 0.38 – 0.42 % Cr (chromium) 0.7 – 0.95 % Fe (iron) 93.4 – 94.8 % Mn (manganese) 0.6 – 0.9 % Mo (molybdenum) 0.3 – 0.45 % Ni (nickel) 1.65 – 2 % P (phosphorus) 0 – 0.01 % S (sulfur) 0 – 0.01 % Si (silicon) 1.5 – 1.8 % V (vanadium) 0.05 – 0.1 %
300M (Low Carbon, Quenched & Tempered Physical properties
300M (Low Carbon, Quenched & Tempered Mechanical properties
Young’s modulus 200 – 210 GPa Specific stiffness 25.5 – 26.9 MN.m/kg Yield strength (elastic limit) 1520 – 1680 MPa Tensile strength 1860 – 2060 MPa Specific strength 194 – 214 kN.m/kg Elongation 8 – 9.3 % strain Compressive strength 1630 – 1800 MPa Flexural modulus 200 – 210 GPa Flexural strength (modulus of rupture) 1520 – 1680 MPa Shear modulus 76 – 79.9 GPa Bulk modulus 185 – 195 GPa Poisson’s ratio 0.32 – 0.333 Shape factor 14 Hardness – Vickers 551 – 609 HV Elastic stored energy (springs) 5610 – 6860 kJ/m3 Fatigue strength at 10^7 cycles 800 – 883 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 754 – 937 MPa
300M (Low Carbon, Quenched & Tempered Impact & fracture properties
Fracture toughness 49.4 – 57.1 MPa.m0.5 Toughness (G) 12 – 15.9 kJ/m2
300M (Low Carbon, Quenched & Tempered Thermal properties
Melting point 1430 – 1510 °C Maximum service temperature 220 – 246 °C Minimum service temperature -73 – -43 °C Thermal conductivity 55 – 59.6 W/m.°C Specific heat capacity 461 – 480 J/kg.°C Thermal expansion coefficient 12.4 – 13.1 µstrain/°C Thermal shock resistance 575 – 649 °C Thermal distortion resistance 4.29 – 4.71 MW/m Latent heat of fusion 265 – 280 kJ/kg
300M (Low Carbon, Quenched & Tempered Electrical properties
Electrical resistivity 18 – 27 µohm.cm Electrical conductivity 6.39 – 9.58 %IACS Galvanic potential -0.49 – -0.41 V
300M (Low Carbon, Quenched & Tempered Magnetic properties
300M (Low Carbon, Quenched & Tempered Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 5050 – 5180 m/s Mechanical loss coefficient (tan delta) 2e-4 – 5e-4
300M (Low Carbon, Quenched & Tempered Processing properties
Metal casting Unsuitable Metal cold forming Excellent Metal hot forming Excellent Metal press forming Excellent Metal deep drawing Limited use Machining speed 7.01 m/min Weldability Notes: Preheating and post weld heat treatments are required Good Carbon equivalency 0.8 – 1
300M (Low Carbon, Quenched & Tempered Durability
Water (fresh) Acceptable Water (salt) Limited use Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Acceptable UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Acceptable Flammability Non-flammable
300M (Low Carbon, Quenched & Tempered Corrosion resistance
Stress corrosion cracking Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments Susceptible
300M (Low Carbon, Quenched & Tempered Notes
300M (Low Carbon, Quenched & Tempered Warning Some rare heat treatments of certain alloys may produce values for mechanical properties outside the given ranges, e.g. AISI 9255. tempered at 205C
300M (Low Carbon, Quenched & Tempered Standards with similar compositions
USA: 300M to SAE J467, 4340M to MIL-S-83135, Grade 8 to ASTM A646-95