AISI 5150 annealed is AISI 5150 low alloy steel (UNS G51500) in the annealed condition. This AISI 5150 annealed material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 5150 conditions in our AISI 5150 yield, tensile and hardness comparison. Looking for AISI 5150 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 5150 steel parts in-house and inspects them before shipment.
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
AISI 5150 Annealed Composition detail
C (carbon)
0.48
–
0.53
%
Cr (chromium)
0.7
–
0.9
%
Fe (iron)
97.2
–
98
%
Mn (manganese)
0.7
–
0.9
%
P (phosphorus)
0
–
0.035
%
S (sulfur)
0
–
0.04
%
Si (silicon)
0.15
–
0.35
%
AISI 5150 Annealed Physical properties
Density
7.8
–
7.9
g/cm3
AISI 5150 Annealed Mechanical properties
Young’s modulus
201
–
212
GPa
Specific stiffness
25.6
–
27
MN.m/kg
Yield strength (elastic limit)
320
–
395
MPa
Tensile strength
605
–
750
MPa
Specific strength
40.8
–
50.3
kN.m/kg
Elongation
17
–
27
% strain
Compressive strength
320
–
395
MPa
Flexural modulus
201
–
212
GPa
Flexural strength (modulus of rupture)
320
–
395
MPa
Shear modulus
77
–
83
GPa
Bulk modulus
155
–
173
GPa
Poisson’s ratio
0.285
–
0.295
Shape factor
57
Hardness – Vickers
160
–
230
HV
Elastic stored energy (springs)
250
–
375
kJ/m3
Fatigue strength at 10^7 cycles
301
–
350
MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
260
–
405
MPa
AISI 5150 Annealed Impact & fracture properties
Fracture toughness
93
–
147
MPa.m0.5
Toughness (G)
43.7
–
100
kJ/m2
AISI 5150 Annealed Thermal properties
Melting point
1410
–
1500
°C
Maximum service temperature
601
–
648
°C
Minimum service temperature
-73
–
-48
°C
Thermal conductivity
42
–
49
W/m.°C
Specific heat capacity
440
–
520
J/kg.°C
Thermal expansion coefficient
12
–
13.5
µstrain/°C
Thermal shock resistance
120
–
153
°C
Thermal distortion resistance
3.24
–
3.92
MW/m
Latent heat of fusion
265
–
280
kJ/kg
AISI 5150 Annealed Electrical properties
Electrical resistivity
21
–
28
µohm.cm
Electrical conductivity
6.16
–
8.21
%IACS
Galvanic potential
-0.5
–
-0.42
V
AISI 5150 Annealed Magnetic properties
Magnetic type
Magnetic
AISI 5150 Annealed Optical, aesthetic and acoustic properties
Transparency
Opaque
Acoustic velocity
5060
–
5200
m/s
Mechanical loss coefficient (tan delta)
7.7e-4
–
9.6e-4
AISI 5150 Annealed Processing properties
Metal casting
Unsuitable
Metal cold forming
Excellent
Metal hot forming
Excellent
Metal press forming
Excellent
Metal deep drawing
Limited use
Machining speed
25.9 m/min
Weldability Notes: Preheating and post weld heat treatments are required
Poor
Carbon equivalency
0.737 – 0.86
AISI 5150 Annealed Durability
Water (fresh)
Acceptable
Water (salt)
Limited use
Weak acids
Limited use
Strong acids
Unacceptable
Weak alkalis
Acceptable
Strong alkalis
Limited use
Organic solvents
Excellent
Oxidation at 500C
Acceptable
UV radiation (sunlight)
Excellent
Galling resistance (adhesive wear)
Acceptable
Flammability
Non-flammable
AISI 5150 Annealed Corrosion resistance
Stress corrosion cracking Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Not susceptible
AISI 5150 Annealed Standards with similar compositions
Australia: 5145 to AS 1444, 5145H to AS 1444, 5150 to AS 1444, 5155 to AS 1444, En11 to AS G18
Czech Republic: 422739 to CSN 422739
India: 50Cr4 to IS 1570/4, 50Cr4 to IS 2507, 50Cr4 to IS 3930, 55Cr3 to IS 13352, 55Cr3 to IS 1570/4, 55Cr70 to IS 1570
Mexico: 5145 to NMX-B-300, 5145H to NMX-B-268, 5145H to NMX-B-300, 5147 to NMX-B-300, 5147H to NMX-B-268, 5147H to NMX-B-300, 5150 to NMX-B-203-SCFI, 5150 to NMX-B-300, 5150H to NMX-B-268, 5150H to NMX-B-300, 5155 to NMX-B-300, 5155H to NMX-B-268, 5155H to NMX-B-300
Pan America: 5150 to COPANT 334
South Korea: SCr 445 to KS D 3707
Sweden: 2230 to SS 142230
USA: 5045, 5145, 5145 to ASTM A29/A29M, 5145 to ASTM A519, 5147, 5147 to ASTM A29/A29M, 5147 to ASTM A519, 5150 to ASTM A29/A29M, 5150 to ASTM A331-95, 5150 to ASTM A519, 5150 to ASTM A866, 5150 to SAE J404, 5150H to ASTM A331-95, 5152, 5155, 5155 to ASTM A29/A29M, 5155 to ASTM A331-95, 5155 to ASTM A519, 6150 to ASTM A331-95, G51500 to ASTM A1031, G51500 to ASTM A506, H51500 to SAE J775, NV6 to SAE J775, UNS G51450, UNS G51470, UNS G51500, UNS G51550, UNS H51450, UNS H51470, UNS H51500, UNS H51550