AISI 4820 normalized is AISI 4820 low alloy steel (UNS G48200) in the normalized condition. This AISI 4820 normalized material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 4820 conditions in our AISI 4820 yield, tensile and hardness comparison. Looking for AISI 4820 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4820 steel parts in-house and inspects them before shipment.
AISI 4820 Normalized Designation
AISI 4820
Condition
Normalized
UNS number
G48200
US name
SAE 4820, ASTM G48200, ASTM 4820, ~ASTM 4820
AISI 4820 Normalized Typical uses
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
AISI 4820 Normalized Composition detail
C (carbon)
0.18
–
0.23
%
Fe (iron)
94.6
–
95.7
%
Mn (manganese)
0.5
–
0.7
%
Mo (molybdenum)
0.2
–
0.3
%
Ni (nickel)
3.25
–
3.75
%
P (phosphorus)
0
–
0.035
%
S (sulfur)
0
–
0.04
%
Si (silicon)
0.15
–
0.35
%
AISI 4820 Normalized Physical properties
Density
7.8
–
7.9
g/cm3
AISI 4820 Normalized Mechanical properties
Young’s modulus
201
–
212
GPa
Specific stiffness
25.6
–
27
MN.m/kg
Yield strength (elastic limit)
435
–
535
MPa
Tensile strength
675
–
830
MPa
Specific strength
55.4
–
68.2
kN.m/kg
Elongation
19
–
29
% strain
Compressive strength
435
–
535
MPa
Flexural modulus
201
–
212
GPa
Flexural strength (modulus of rupture)
435
–
535
MPa
Shear modulus
77
–
83
GPa
Bulk modulus
155
–
173
GPa
Poisson’s ratio
0.285
–
0.295
Shape factor
48
Hardness – Vickers
210
–
260
HV
Elastic stored energy (springs)
462
–
688
kJ/m3
Fatigue strength at 10^7 cycles
325
–
376
MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
282
–
433
MPa
AISI 4820 Normalized Impact & fracture properties
Fracture toughness
72
–
115
MPa.m0.5
Toughness (G)
26.2
–
61.3
kJ/m2
AISI 4820 Normalized Thermal properties
Melting point
1480
–
1520
°C
Maximum service temperature
638
–
660
°C
Minimum service temperature
-73
–
-43
°C
Thermal conductivity
35
–
50
W/m.°C
Specific heat capacity
460
–
500
J/kg.°C
Thermal expansion coefficient
10.5
–
13
µstrain/°C
Thermal shock resistance
173
–
232
°C
Thermal distortion resistance
2.92
–
4.39
MW/m
Latent heat of fusion
265
–
280
kJ/kg
AISI 4820 Normalized Electrical properties
Electrical resistivity
23
–
29
µohm.cm
Electrical conductivity
5.95
–
7.5
%IACS
Galvanic potential
-0.51
–
-0.43
V
AISI 4820 Normalized Magnetic properties
Magnetic type
Magnetic
AISI 4820 Normalized Optical, aesthetic and acoustic properties
Transparency
Opaque
Acoustic velocity
5060
–
5200
m/s
Mechanical loss coefficient (tan delta)
6.3e-4
–
7.8e-4
AISI 4820 Normalized Processing properties
Metal casting
Unsuitable
Metal cold forming
Excellent
Metal hot forming
Excellent
Metal press forming
Excellent
Metal deep drawing
Limited use
Machining speed
20.1 m/min
Weldability Notes: Preheating and post weld heat treatments may be required
Good
Carbon equivalency
0.52 – 0.657
AISI 4820 Normalized Durability
Water (fresh)
Acceptable
Water (salt)
Limited use
Weak acids
Limited use
Strong acids
Unacceptable
Weak alkalis
Acceptable
Strong alkalis
Limited use
Organic solvents
Excellent
Oxidation at 500C
Acceptable
UV radiation (sunlight)
Excellent
Galling resistance (adhesive wear)
Acceptable
Flammability
Non-flammable
AISI 4820 Normalized Corrosion resistance
Stress corrosion cracking Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible
AISI 4820 Normalized Standards with similar compositions
Argentina: IRAM 4815 to IAS
Mexico: 4815 to NMX-B-203-SCFI, 4815 to NMX-B-300, 4817 to NMX-B-203-SCFI, 4817 to NMX-B-300, 4817H to NMX-B-268, 4817H to NMX-B-300, 4820 to NMX-B-203-SCFI, 4820 to NMX-B-300, 4820H to NMX-B-268, 4820H to NMX-B-300
Pan America: 4817 to COPANT 334, 4820 to COPANT 514
Romania: 20MoNi35 to STAS 791, 20MoNi35S to STAS 791, 20MoNi35X to STAS 791, 20MoNi35XS to STAS 791
USA: 4815 to ASTM A29/A29M, 4815 to ASTM A331-95, 4815 to ASTM A519, 4815 to SAE J770, 4817, 4817 to ASTM A29/A29M, 4817 to ASTM A331-95, 4817 to ASTM A519, 4817 to SAE J770, 4817H to ASTM A534, 4820, 4820 to ASTM A29/A29M, 4820 to ASTM A322-91, 4820 to ASTM A331-95, 4820 to ASTM A519, 4820 to ASTM A752/A752M, 4820 to SAE J404, 4820H, 4820H to ASTM A304, 4820H to ASTM A331-95, 4820H to ASTM A534, 4820H to SAE J1268, 4820RH to ASTM A914/A914M-92, 4820RH to SAE J1868, G48150 to ASTM A1031, G48200 to ASTM A1031, UNS G48150, UNS G48170, UNS G48200, UNS H48170, UNS H48200