AISI 4820 Annealed Material Data Sheet

AISI 4820 Annealed Material Data Sheet

AISI 4820 Annealed Overview

AISI 4820 annealed is AISI 4820 low alloy steel (UNS G48200) in the annealed condition. This AISI 4820 annealed material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 4820 conditions in our AISI 4820 yield, tensile and hardness comparison. Looking for AISI 4820 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4820 steel parts in-house and inspects them before shipment.

AISI 4820 Annealed Designation

AISI 4820
ConditionAnnealed
UNS numberG48200
US nameSAE 4820, ASTM G48200, ASTM 4820, ~ASTM 4820

AISI 4820 Annealed Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 4820 Annealed Composition detail

C (carbon)0.18–0.23%
Fe (iron)94.6–95.7%
Mn (manganese)0.5–0.7%
Mo (molybdenum)0.2–0.3%
Ni (nickel)3.25–3.75%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 4820 Annealed Physical properties

Density7.8–7.9g/cm3

AISI 4820 Annealed Mechanical properties

Young’s modulus201–212GPa
Specific stiffness25.6–27MN.m/kg
Yield strength (elastic limit)410–515MPa
Tensile strength610–750MPa
Specific strength52.2–65.6kN.m/kg
Elongation18–27% strain
Compressive strength410–515MPa
Flexural modulus201–212GPa
Flexural strength (modulus of rupture)410–515MPa
Shear modulus77–83GPa
Bulk modulus155–173GPa
Poisson’s ratio0.285–0.295 
Shape factor50
Hardness – Vickers183–223HV
Elastic stored energy (springs)411–636kJ/m3
Fatigue strength at 10^7 cycles302–350MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
263–402MPa

AISI 4820 Annealed Impact & fracture properties

Fracture toughness68–111MPa.m0.5
Toughness (G)23.5–56.9kJ/m2

AISI 4820 Annealed Thermal properties

Melting point1480–1520°C
Maximum service temperature638–660°C
Minimum service temperature-73–-48°C
Thermal conductivity35–50W/m.°C
Specific heat capacity460–500J/kg.°C
Thermal expansion coefficient10.5–13µstrain/°C
Thermal shock resistance163–222°C
Thermal distortion resistance2.92–4.39MW/m
Latent heat of fusion265–280kJ/kg

AISI 4820 Annealed Electrical properties

Electrical resistivity23–29µohm.cm
Electrical conductivity5.95–7.5%IACS
Galvanic potential-0.51–-0.43V

AISI 4820 Annealed Magnetic properties

Magnetic typeMagnetic

AISI 4820 Annealed Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5200m/s
Mechanical loss coefficient (tan delta)6.7e-4–8.4e-4 

AISI 4820 Annealed Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed22.9 m/min
Weldability
Notes: Preheating and post weld heat treatments may be required
Good
Carbon equivalency0.52 – 0.657

AISI 4820 Annealed Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 4820 Annealed Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 4820 Annealed Standards with similar compositions

Argentina: IRAM 4815 to IAS
Mexico: 4815 to NMX-B-203-SCFI, 4815 to NMX-B-300, 4817 to NMX-B-203-SCFI, 4817 to NMX-B-300, 4817H to NMX-B-268, 4817H to NMX-B-300, 4820 to NMX-B-203-SCFI, 4820 to NMX-B-300, 4820H to NMX-B-268, 4820H to NMX-B-300
Pan America: 4817 to COPANT 334, 4820 to COPANT 514
Romania: 20MoNi35 to STAS 791, 20MoNi35S to STAS 791, 20MoNi35X to STAS 791, 20MoNi35XS to STAS 791
USA: 4815 to ASTM A29/A29M, 4815 to ASTM A331-95, 4815 to ASTM A519, 4815 to SAE J770, 4817, 4817 to ASTM A29/A29M, 4817 to ASTM A331-95, 4817 to ASTM A519, 4817 to SAE J770, 4817H to ASTM A534, 4820, 4820 to ASTM A29/A29M, 4820 to ASTM A322-91, 4820 to ASTM A331-95, 4820 to ASTM A519, 4820 to ASTM A752/A752M, 4820 to SAE J404, 4820H, 4820H to ASTM A304, 4820H to ASTM A331-95, 4820H to ASTM A534, 4820H to SAE J1268, 4820RH to ASTM A914/A914M-92, 4820RH to SAE J1868, G48150 to ASTM A1031, G48200 to ASTM A1031, UNS G48150, UNS G48170, UNS G48200, UNS H48170, UNS H48200