AISI 4340 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 205°C Overview

AISI 4340 tempered 205°C is AISI 4340 low alloy steel (UNS G43400) in the oil quenched & tempered at 205°C condition. This AISI 4340 tempered 205°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 4340 conditions in our AISI 4340 yield, tensile and hardness comparison. Looking for AISI 4340 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4340 steel parts in-house and inspects them before shipment.

AISI 4340 Oil Quenched & Tempered at 205°C Designation

AISI 4340
ConditionTempered at 205°C & oil quenched
UNS numberG43400
US nameSAE E4340, SAE 4340, SAE E4340, SAE 4340H, SAE 4340, SAE 4330H, ASTM E4340, ASTM 4340, ASTM G43406, ASTM G43400, ASTM E4340H, ASTM E4340, ASTM 1B 1, ASTM B24V, ASTM B23, ASTM 4340H, ASTM 4340, ASTM 4 G, ASME E4340, ~SAE E4340H, ~ASTM B24
GB (Chinese) name~ 40CrNiMoA
JIS (Japanese) nameSNCM447RCH, SNCM 439, SNB24-5, SNB24-4, SNB24-3, SNB24-2, SNB23-1, ~ SNCM 439, ~SNCM439RCH, ~SNB24-1, ~SNB23-5, ~SNB23-4, ~SNB23-3, ~SNB23-2

AISI 4340 Oil Quenched & Tempered at 205°C Typical uses

High tensile applications, general engineering parts, through-hardened gears, connecting rods and bolts, gun barrels

AISI 4340 Oil Quenched & Tempered at 205°C Composition detail

C (carbon)0.38–0.43%
Cr (chromium)0.7–0.9%
Fe (iron)95.2–96.3%
Mn (manganese)0.6–0.8%
Mo (molybdenum)0.2–0.3%
Ni (nickel)1.65–2%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.3%

AISI 4340 Oil Quenched & Tempered at 205°C Physical properties

Density7.8–7.9g/cm3

AISI 4340 Oil Quenched & Tempered at 205°C Mechanical properties

Young’s modulus205–213GPa
Specific stiffness26.1–27.2MN.m/kg
Yield strength (elastic limit)1510–1850MPa
Tensile strength1580–2070MPa
Specific strength192–235kN.m/kg
Elongation8–12% strain
Compressive strength1510–1850MPa
Flexural modulus205–213GPa
Flexural strength (modulus of rupture)1510–1850MPa
Shear modulus79–83GPa
Bulk modulus158–174GPa
Poisson’s ratio0.285–0.295 
Shape factor14
Hardness – Vickers465–575HV
Elastic stored energy (springs)5470–8070kJ/m3
Fatigue strength at 10^7 cycles589–712MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
497–845MPa

AISI 4340 Oil Quenched & Tempered at 205°C Impact & fracture properties

Fracture toughness44–66MPa.m0.5
Toughness (G)9.58–20.1kJ/m2

AISI 4340 Oil Quenched & Tempered at 205°C Thermal properties

Melting point1430–1510°C
Maximum service temperature165–195°C
Minimum service temperature-48–-23°C
Thermal conductivity35–50W/m.°C
Specific heat capacity440–520J/kg.°C
Thermal expansion coefficient11.5–13µstrain/°C
Thermal shock resistance579–734°C
Thermal distortion resistance2.84–4.12MW/m
Latent heat of fusion265–280kJ/kg

AISI 4340 Oil Quenched & Tempered at 205°C Electrical properties

Electrical resistivity18–27µohm.cm
Electrical conductivity6.39–9.58%IACS
Galvanic potential-0.5–-0.42V

AISI 4340 Oil Quenched & Tempered at 205°C Magnetic properties

Magnetic typeMagnetic

AISI 4340 Oil Quenched & Tempered at 205°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5110–5210m/s
Mechanical loss coefficient (tan delta)2.1e-4–2.8e-4 

AISI 4340 Oil Quenched & Tempered at 205°C Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed8.23 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Good
Carbon equivalency0.77 – 0.937

AISI 4340 Oil Quenched & Tempered at 205°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 4340 Oil Quenched & Tempered at 205°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Susceptible

AISI 4340 Oil Quenched & Tempered at 205°C Notes

AISI 4340 Oil Quenched & Tempered at 205°C Other notes
A very popular, versatile steel. It can be heat-treated to produce a wide range of tensile strengths in moderate sections.

AISI 4340 Oil Quenched & Tempered at 205°C Standards with similar compositions

Argentina: IRAM 4340 to IAS
Australia: 4340 to AS 1444, 4340H to AS 1444
Germany: 40NiCrMo73 to DIN
International: 4 to ISO 683-8, 41NiCrMo7E to ISO 4954, 4A to ISO 683-8, 4b to ISO 683-8
Italy: 40NiCrMo7 to UNI 5332, 40NiCrMo7 to UNI 7845, 40NiCrMo7 to UNI 7874, 40NiCrMo7KB to UNI 7356
Japan: SNB23-1 to JIS G4108, SNB23-2 to JIS G4108, SNB23-3 to JIS G4108, SNB23-4 to JIS G4108, SNB23-5 to JIS G4108, SNB24-1 to JIS G4108, SNB24-2 to JIS G4108, SNB24-3 to JIS G4108, SNB24-4 to JIS G4108, SNB24-5 to JIS G4108, SNCM 439 to JIS G4053, SNCM439 to JIS G4103, SNCM439RCH to JIS G3509-1, SNCM8 to JIS G4103
Mexico: 4340 to NMX-B-203-SCFI, 4340 to NMX-B-300, 4340H to NMX-B-268, 4340H to NMX-B-300, E4340 to NMX-B-203-SCFI, E4340 to NMX-B-300, E4340H to NMX-B-268, E4340H to NMX-B-300
Pan America: 4340 to COPANT 334, 4340 to COPANT 514, E4340 to COPANT 514
South Korea: SNCM 439 to KS D 3709
Spain: 35NiCrMo7 to UNE 36012, 40NiCrMo7 to UNE 36012, F.1270 to UNE 36012, F.1272 to UNE 36012
USA: 4337, 4337 to ASTM A519, 4340, 4340 to ASTM A29/A29M, 4340 to ASTM A322-91, 4340 to ASTM A331-95, 4340 to ASTM A519, 4340 to ASTM A752/A752M, 4340 to ASTM A829/A829M, 4340 to DoD-F-24669/1, 4340 to FED QQ-S-626C, 4340 to SAE J404, 4340H, 4340H to ASTM A304, 4340H to ASTM A331-95, 4340H to SAE J1268, B23 to ASTM A540/A540M, B24 to ASTM A540/A540M, E4337 to ASTM A519, E4340, E4340 to ASTM A29/A29M, E4340 to ASTM A322-91, E4340 to ASTM A331-95, E4340 to ASTM A519, E4340 to ASTM A752/A752M, E4340 to ASTM A829/A829M, E4340 to SAE J404, E4340 to SAE J770, G43400 to ASTM A1031, G43400 to ASTM A506, G43400 to MIL-S-46059, G43406 to ASTM A1031, Grade 7 to ASTM A646-95, Grade L to ASTM A372/A372M, L43 to ASTM A320/A320M, UNS G43370, UNS G43376, UNS G43400, UNS G43406, UNS H43400, UNS H43406, UNS K24040, UNS K24045, UNS K24055, UNS K24064
Tradenames: 40 NI CR MO 7, A-1272, CROMETEX NO. 1, LESCALLOY 4340 VAC-ARC, POMPEY 4.340, VASCO 4340, VM-40