AISI 4340 Quenched & Tempered Material Data Sheet
AISI 4340 Quenched & Tempered Overview
| AISI 4340 quenched tempered is AISI 4340 low alloy steel (UNS G43400) in the quenched & tempered condition. This AISI 4340 quenched tempered material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 4340 conditions in our AISI 4340 yield, tensile and hardness comparison. Looking for AISI 4340 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4340 steel parts in-house and inspects them before shipment. |
AISI 4340 Quenched & Tempered Designation
| AISI 4340 | |
| Condition | Quenched & tempered |
| UNS number | G43400 |
| US name | SAE E4340, SAE 4340, SAE E4340, SAE 4340H, SAE 4340, SAE 4330H, ASTM E4340, ASTM 4340, ASTM G43406, ASTM G43400, ASTM E4340H, ASTM E4340, ASTM 1B 1, ASTM B24V, ASTM B23, ASTM 4340H, ASTM 4340, ASTM 4 G, ASME E4340, ~SAE E4340H, ~ASTM B24 |
| GB (Chinese) name | ~ 40CrNiMoA |
| JIS (Japanese) name | SNCM447RCH, SNCM 439, SNB24-5, SNB24-4, SNB24-3, SNB24-2, SNB23-1, ~ SNCM 439, ~SNCM439RCH, ~SNB24-1, ~SNB23-5, ~SNB23-4, ~SNB23-3, ~SNB23-2 |
AISI 4340 Quenched & Tempered Typical uses
| General construction, general mechanical engineering, automotive, pressure vessels, pipework |
AISI 4340 Quenched & Tempered Composition detail
| C (carbon) | 0.38 | – | 0.43 | % |
| Cr (chromium) | 0.7 | – | 0.9 | % |
| Fe (iron) | 95.2 | – | 96.3 | % |
| Mn (manganese) | 0.6 | – | 0.8 | % |
| Mo (molybdenum) | 0.2 | – | 0.3 | % |
| Ni (nickel) | 1.65 | – | 2 | % |
| P (phosphorus) | 0 | – | 0.035 | % |
| S (sulfur) | 0 | – | 0.04 | % |
| Si (silicon) | 0.15 | – | 0.3 | % |
AISI 4340 Quenched & Tempered Physical properties
| Density | 7.79 | – | 7.87 | g/cm3 |
AISI 4340 Quenched & Tempered Mechanical properties
| Young’s modulus | 200 | – | 210 | GPa |
| Specific stiffness | 25.5 | – | 26.9 | MN.m/kg |
| Yield strength (elastic limit) | 1500 | – | 1650 | MPa |
| Tensile strength | 1790 | – | 1980 | MPa |
| Specific strength | 191 | – | 211 | kN.m/kg |
| Elongation | 8 | – | 10 | % strain |
| Compressive strength | 1620 | – | 1790 | MPa |
| Flexural modulus | 200 | – | 210 | GPa |
| Flexural strength (modulus of rupture) | 1500 | – | 1650 | MPa |
| Shear modulus | 76 | – | 79.9 | GPa |
| Bulk modulus | 185 | – | 195 | GPa |
| Poisson’s ratio | 0.32 | – | 0.333 | |
| Shape factor | 15 | |||
| Hardness – Vickers | 385 | – | 475 | HV |
| Elastic stored energy (springs) | 5450 | – | 6670 | kJ/m3 |
| Fatigue strength at 10^7 cycles | 519 | – | 600 | MPa |
| Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 495 | – | 629 | MPa |
AISI 4340 Quenched & Tempered Impact & fracture properties
| Fracture toughness | 79 | – | 91 | MPa.m0.5 |
| Toughness (G) | 30.5 | – | 40.3 | kJ/m2 |
AISI 4340 Quenched & Tempered Thermal properties
| Melting point | 1430 | – | 1510 | °C |
| Maximum service temperature | 160 | – | 180 | °C |
| Minimum service temperature | -58 | – | -28 | °C |
| Thermal conductivity | 36.3 | – | 39.3 | W/m.°C |
| Specific heat capacity | 461 | – | 480 | J/kg.°C |
| Thermal expansion coefficient | 12.4 | – | 13.1 | µstrain/°C |
| Thermal shock resistance | 567 | – | 640 | °C |
| Thermal distortion resistance | 2.83 | – | 3.11 | MW/m |
| Latent heat of fusion | 265 | – | 280 | kJ/kg |
AISI 4340 Quenched & Tempered Electrical properties
| Electrical resistivity | 18 | – | 27 | µohm.cm |
| Electrical conductivity | 6.39 | – | 9.58 | %IACS |
| Galvanic potential | -0.5 | – | -0.42 | V |
AISI 4340 Quenched & Tempered Magnetic properties
| Magnetic type | Magnetic |
AISI 4340 Quenched & Tempered Optical, aesthetic and acoustic properties
| Transparency | Opaque | |||
| Acoustic velocity | 5050 | – | 5180 | m/s |
| Mechanical loss coefficient (tan delta) | 2e-4 | – | 5e-4 | |
AISI 4340 Quenched & Tempered Processing properties
| Metal casting | Unsuitable |
| Metal cold forming | Excellent |
| Metal hot forming | Excellent |
| Metal press forming | Excellent |
| Metal deep drawing | Limited use |
| Machining speed | 9.45 m/min |
| Weldability Notes: Preheating and post weld heat treatments are required | Good |
| Carbon equivalency | 0.77 – 0.937 |
AISI 4340 Quenched & Tempered Durability
| Water (fresh) | Acceptable |
| Water (salt) | Limited use |
| Weak acids | Limited use |
| Strong acids | Unacceptable |
| Weak alkalis | Acceptable |
| Strong alkalis | Limited use |
| Organic solvents | Excellent |
| Oxidation at 500C | Acceptable |
| UV radiation (sunlight) | Excellent |
| Galling resistance (adhesive wear) | Acceptable |
| Flammability | Non-flammable |
AISI 4340 Quenched & Tempered Corrosion resistance
| Stress corrosion cracking Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments | Susceptible |
AISI 4340 Quenched & Tempered Notes
| AISI 4340 Quenched & Tempered Warning |
| Some rare heat treatments of certain alloys may produce values for mechanical properties outside the given ranges, e.g. AISI 9255. tempered at 205C |
AISI 4340 Quenched & Tempered Standards with similar compositions
| Argentina: IRAM 4340 to IAS |
| Australia: 4340 to AS 1444, 4340H to AS 1444 |
| Germany: 40NiCrMo73 to DIN |
| International: 4 to ISO 683-8, 41NiCrMo7E to ISO 4954, 4A to ISO 683-8, 4b to ISO 683-8 |
| Italy: 40NiCrMo7 to UNI 5332, 40NiCrMo7 to UNI 7845, 40NiCrMo7 to UNI 7874, 40NiCrMo7KB to UNI 7356 |
| Japan: SNB23-1 to JIS G4108, SNB23-2 to JIS G4108, SNB23-3 to JIS G4108, SNB23-4 to JIS G4108, SNB23-5 to JIS G4108, SNB24-1 to JIS G4108, SNB24-2 to JIS G4108, SNB24-3 to JIS G4108, SNB24-4 to JIS G4108, SNB24-5 to JIS G4108, SNCM 439 to JIS G4053, SNCM439 to JIS G4103, SNCM439RCH to JIS G3509-1, SNCM8 to JIS G4103 |
| Mexico: 4340 to NMX-B-203-SCFI, 4340 to NMX-B-300, 4340H to NMX-B-268, 4340H to NMX-B-300, E4340 to NMX-B-203-SCFI, E4340 to NMX-B-300, E4340H to NMX-B-268, E4340H to NMX-B-300 |
| Pan America: 4340 to COPANT 334, 4340 to COPANT 514, E4340 to COPANT 514 |
| South Korea: SNCM 439 to KS D 3709 |
| Spain: 35NiCrMo7 to UNE 36012, 40NiCrMo7 to UNE 36012, F.1270 to UNE 36012, F.1272 to UNE 36012 |
| USA: 4337, 4337 to ASTM A519, 4340, 4340 to ASTM A29/A29M, 4340 to ASTM A322-91, 4340 to ASTM A331-95, 4340 to ASTM A519, 4340 to ASTM A752/A752M, 4340 to ASTM A829/A829M, 4340 to DoD-F-24669/1, 4340 to FED QQ-S-626C, 4340 to SAE J404, 4340H, 4340H to ASTM A304, 4340H to ASTM A331-95, 4340H to SAE J1268, B23 to ASTM A540/A540M, B24 to ASTM A540/A540M, E4337 to ASTM A519, E4340, E4340 to ASTM A29/A29M, E4340 to ASTM A322-91, E4340 to ASTM A331-95, E4340 to ASTM A519, E4340 to ASTM A752/A752M, E4340 to ASTM A829/A829M, E4340 to SAE J404, E4340 to SAE J770, G43400 to ASTM A1031, G43400 to ASTM A506, G43400 to MIL-S-46059, G43406 to ASTM A1031, Grade 7 to ASTM A646-95, Grade L to ASTM A372/A372M, L43 to ASTM A320/A320M, UNS G43370, UNS G43376, UNS G43400, UNS G43406, UNS H43400, UNS H43406, UNS K24040, UNS K24045, UNS K24055, UNS K24064 |
| Tradenames: 40 NI CR MO 7, A-1272, CROMETEX NO. 1, LESCALLOY 4340 VAC-ARC, POMPEY 4.340, VASCO 4340, VM-40 |