D6AC Low Alloy Steel

D6AC Low Alloy Steel

D6AC Steel Overview

D6AC steel (UNS K24728) is a low alloy steel. This page lists the D6AC material data sheets for 1 condition: quenched & tempered. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of D6AC Steel

General construction, general mechanical engineering, automotive, pressure vessels, pipework

D6AC Steel Chemical Composition

C (carbon)0.45 – 0.5 %
Cr (chromium)0.9 – 1.2 %
Fe (iron)95.1 – 96.5 %
Mn (manganese)0.6 – 0.9 %
Mo (molybdenum)0.9 – 1.1 %
Ni (nickel)0.4 – 0.7 %
P (phosphorus)0 – 0.01 %
S (sulfur)0 – 0.01 %
Si (silicon)0.15 – 0.3 %
V (vanadium)0.08 – 0.15 %

D6AC Steel Material Data Sheets

D6AC Quenched & Tempered Material Data Sheet

D6AC Steel Parts from Turkey

Looking for D6AC parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined D6AC steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.