4335V Low Alloy Steel

4335V Low Alloy Steel

4335V Steel Overview

4335V steel (UNS K33517, EN 38NiCrMoV7-3) is a low alloy steel. This page lists the 4335V material data sheets for 1 condition: quenched & tempered. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of 4335V Steel

General construction, general mechanical engineering, automotive, pressure vessels, pipework

4335V Steel Chemical Composition

C (carbon)0.32 – 0.38 %
Cr (chromium)0.65 – 0.9 %
Fe (iron)94.6 – 96.1 %
Mn (manganese)0.6 – 0.9 %
Mo (molybdenum)0.3 – 0.4 %
Ni (nickel)1.65 – 2 %
S (sulfur)0 – 0.04 %
Si (silicon)0.2 – 0.6 %
V (vanadium)0.17 – 0.23 %

4335V Steel Material Data Sheets

4335V Quenched & Tempered Material Data Sheet

4335V Steel Parts from Turkey

Looking for 4335V parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined 4335V steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.