AISI 8735 Low Alloy Steel

AISI 8735 Low Alloy Steel

AISI 8735 Steel Overview

AISI 8735 steel (UNS G87350) is a low alloy steel. This page lists the AISI 8735 material data sheets for 1 condition: normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 8735 Steel

General construction, general mechanical engineering, automotive, pressure vessels, pipework

AISI 8735 Steel Chemical Composition

C (carbon)0.33 – 0.38 %
Cr (chromium)0.4 – 0.6 %
Fe (iron)96.6 – 97.8 %
Mn (manganese)0.75 – 1 %
Mo (molybdenum)0.2 – 0.3 %
Ni (nickel)0.4 – 0.7 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %