AISI 6150 Low Alloy Steel

AISI 6150 Low Alloy Steel

AISI 6150 Steel Overview

AISI 6150 steel (UNS G61500, EN 51CrMnV4) is a low alloy steel. This page lists the AISI 6150 material data sheets for 7 conditions: annealed, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 6150 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 6150 Steel Chemical Composition

C (carbon)0.48 – 0.53 %
Cr (chromium)0.8 – 1.1 %
Fe (iron)96.9 – 97.7 %
Mn (manganese)0.7 – 0.9 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %
V (vanadium)0.15 %

AISI 6150 Steel Material Data Sheets

AISI 6150 Annealed Material Data Sheet

AISI 6150 Normalized Material Data Sheet

AISI 6150 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 6150 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 6150 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 6150 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 6150 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 6150 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 6150 Annealed vs Normalized vs Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 6150 Steel Parts from Turkey

Looking for AISI 6150 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 6150 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.