AISI 5160 steel (UNS G51600) is a low alloy steel. This page lists the AISI 5160 material data sheets for 7 conditions: annealed, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 5160 Steel
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
Looking for AISI 5160 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 5160 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.