AISI 5130 Low Alloy Steel

AISI 5130 Low Alloy Steel

AISI 5130 Steel Overview

AISI 5130 steel (UNS G51300, EN 34Cr4) is a low alloy steel. This page lists the AISI 5130 material data sheets for 5 conditions: oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 5130 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 5130 Steel Chemical Composition

C (carbon)0.28 – 0.33 %
Cr (chromium)0.8 – 1.1 %
Fe (iron)97.2 – 98.1 %
Mn (manganese)0.7 – 0.9 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 5130 Steel Material Data Sheets

AISI 5130 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 5130 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 5130 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 5130 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 5130 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 5130 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 5130 Tempering Temperature Comparison (205–650°C): Yield, Tensile & Hardness.