AISI 5130 Oil Quenched & Tempered at 205°C Material Data Sheet
AISI 5130 Oil Quenched & Tempered at 205°C Overview
| AISI 5130 tempered 205°C is AISI 5130 low alloy steel (UNS G51300, EN 34Cr4) in the oil quenched & tempered at 205°C condition. This AISI 5130 tempered 205°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 5130 conditions in our AISI 5130 yield, tensile and hardness comparison. Looking for AISI 5130 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 5130 steel parts in-house and inspects them before shipment. |
AISI 5130 Oil Quenched & Tempered at 205°C Designation
| AISI 5130 | |
| Condition | Tempered at 205°C & oil quenched |
| UNS number | G51300 |
| US name | SAE 5130, SAE 5132H, SAE 5132, ASTM 5130, ASTM G51300, ASTM 5132H, ASTM 5132, ASTM 5130H, ASTM 5130, ~ASTM 5130 |
| EN name | ~34CrS4, ~34Cr4, ~28Cr4 |
| EN number | ~1.7037, ~1.7033, ~1.703 |
| ISO name | 34CrS4, 34Cr4, 1b, ~34Cr4 |
| GB (Chinese) name | ~30CrMnSiA |
AISI 5130 Oil Quenched & Tempered at 205°C Typical uses
| General construction, general mechanical engineering, automotive, tools, axles, gears, springs. |
AISI 5130 Oil Quenched & Tempered at 205°C Composition detail
| C (carbon) | 0.28 | – | 0.33 | % |
| Cr (chromium) | 0.8 | – | 1.1 | % |
| Fe (iron) | 97.2 | – | 98.1 | % |
| Mn (manganese) | 0.7 | – | 0.9 | % |
| P (phosphorus) | 0 | – | 0.035 | % |
| S (sulfur) | 0 | – | 0.04 | % |
| Si (silicon) | 0.15 | – | 0.35 | % |
AISI 5130 Oil Quenched & Tempered at 205°C Physical properties
| Density | 7.8 | – | 7.9 | g/cm3 |
AISI 5130 Oil Quenched & Tempered at 205°C Mechanical properties
| Young’s modulus | 201 | – | 217 | GPa |
| Specific stiffness | 25.6 | – | 27.7 | MN.m/kg |
| Yield strength (elastic limit) | 1370 | – | 1670 | MPa |
| Tensile strength | 1460 | – | 1780 | MPa |
| Specific strength | 174 | – | 213 | kN.m/kg |
| Elongation | 8 | – | 12 | % strain |
| Compressive strength | 1370 | – | 1670 | MPa |
| Flexural modulus | 201 | – | 217 | GPa |
| Flexural strength (modulus of rupture) | 1370 | – | 1670 | MPa |
| Shear modulus | 77 | – | 85 | GPa |
| Bulk modulus | 155 | – | 177 | GPa |
| Poisson’s ratio | 0.285 | – | 0.295 | |
| Shape factor | 15 | |||
| Hardness – Vickers | 425 | – | 525 | HV |
| Elastic stored energy (springs) | 4490 | – | 6630 | kJ/m3 |
| Fatigue strength at 10^7 cycles | 556 | – | 641 | MPa |
| Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 487 | – | 732 | MPa |
AISI 5130 Oil Quenched & Tempered at 205°C Impact & fracture properties
| Fracture toughness | 27 | – | 50 | MPa.m0.5 |
| Toughness (G) | 3.75 | – | 11.1 | kJ/m2 |
AISI 5130 Oil Quenched & Tempered at 205°C Thermal properties
| Melting point | 1460 | – | 1510 | °C |
| Maximum service temperature | 165 | – | 195 | °C |
| Minimum service temperature | -53 | – | -28 | °C |
| Thermal conductivity | 45 | – | 50 | W/m.°C |
| Specific heat capacity | 470 | – | 530 | J/kg.°C |
| Thermal expansion coefficient | 11.5 | – | 13 | µstrain/°C |
| Thermal shock resistance | 523 | – | 668 | °C |
| Thermal distortion resistance | 3.58 | – | 4.2 | MW/m |
| Latent heat of fusion | 265 | – | 280 | kJ/kg |
AISI 5130 Oil Quenched & Tempered at 205°C Electrical properties
| Electrical resistivity | 18 | – | 24 | µohm.cm |
| Electrical conductivity | 7.18 | – | 9.58 | %IACS |
| Galvanic potential | -0.5 | – | -0.42 | V |
AISI 5130 Oil Quenched & Tempered at 205°C Magnetic properties
| Magnetic type | Magnetic |
AISI 5130 Oil Quenched & Tempered at 205°C Optical, aesthetic and acoustic properties
| Transparency | Opaque | |||
| Acoustic velocity | 5060 | – | 5260 | m/s |
| Mechanical loss coefficient (tan delta) | 2.4e-4 | – | 3e-4 | |
AISI 5130 Oil Quenched & Tempered at 205°C Processing properties
| Metal casting | Unsuitable |
| Metal cold forming | Excellent |
| Metal hot forming | Excellent |
| Metal press forming | Excellent |
| Metal deep drawing | Limited use |
| Machining speed | 10.1 m/min |
| Weldability Notes: Preheating and post weld heat treatments are required | Good |
| Carbon equivalency | 0.557 – 0.7 |
AISI 5130 Oil Quenched & Tempered at 205°C Durability
| Water (fresh) | Acceptable |
| Water (salt) | Limited use |
| Weak acids | Limited use |
| Strong acids | Unacceptable |
| Weak alkalis | Acceptable |
| Strong alkalis | Limited use |
| Organic solvents | Excellent |
| Oxidation at 500C | Acceptable |
| UV radiation (sunlight) | Excellent |
| Galling resistance (adhesive wear) | Acceptable |
| Flammability | Non-flammable |
AISI 5130 Oil Quenched & Tempered at 205°C Corrosion resistance
| Stress corrosion cracking Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments | Susceptible |
AISI 5130 Oil Quenched & Tempered at 205°C Standards with similar compositions
| Argentina: IRAM 5130 to IAS, IRAM 5132 to IAS |
| Australia: 5132 to AS 1444, 5132H to AS 1444 |
| Belgium: 34Cr4 to NBN 251 |
| China: 30Cr to GB/T 11251 |
| France: 32C4 to AFNOR NF A35-552, 32C4 to AFNOR NF A35-553, 32C4 to AFNOR NF A35-556, 32C4 to AFNOR NF A35-557 |
| Germany: 1.7030 to DIN EN 10083, 1.7033 to DIN 1652, 1.7033 to DIN EN 10083, 1.7037 to DIN EN 10083, 28Cr4 to DIN EN 10083, 34Cr4 to DIN 1652, 34Cr4 to DIN EN 10083, 34CrS4 to DIN EN 10083 |
| Hungary: Cr1 to MSZ 61, Cr1E to MSZ 61, Cr1Z to MSZ 6251 |
| International: 1 to ISO 683-7, 1a to ISO 683-7, 1b to ISO 683-7, 34Cr4 to ISO 683-1, 34Cr4 to ISO 683-18, 34Cr4E to ISO 4954, 34CrS4 to ISO 683-1, 34CrS4 to ISO 683-18 |
| Italy: 34Cr4 to UNI 7874, 34Cr4KB to UNI 7356 |
| Japan: SCr2H to JIS G4052, SCr3H to JIS G4052, SCr430HRCH to JIS G3509-1, SCr430RCH to JIS G3509-1 |
| Mexico: 5130 to NMX-B-203-SCFI, 5130 to NMX-B-300, 5130H to NMX-B-268, 5130H to NMX-B-300, 5132 to NMX-B-203-SCFI, 5132 to NMX-B-300, 5132H to NMX-B-268, 5132H to NMX-B-300, 5135 to NMX-B-300, 5135H to NMX-B-268, 5135H to NMX-B-300 |
| Pan America: 5130 to COPANT 334, 5135 to COPANT 334 |
| Romania: 32Cr10 to STAS 11500/2 |
| South Korea: SCr 430 H to KS D 3754, SCr 430 to KS D 3707, SCr 435 H to KS D 3754, SCr 435 to KS D 3707 |
| UK: 28Cr4 to BS EN 10084, 28CrS4 to BS EN 10084, 34Cr4 to BS EN 10083-1, 34Cr4 to BS EN 10250-3, 34CrS4 to BS EN 10083-1, 34CrS4 to BS EN 10277-5 |
| USA: 5130 to ASTM A29/A29M, 5130 to ASTM A331-95, 5130 to ASTM A513, 5130 to ASTM A519, 5130 to SAE J404, 5132 to ASTM A29/A29M, 5132 to ASTM A331-95, 5132 to ASTM A519, 5132 to SAE J404, 5132 to SAE J770, 5135, 5135 to ASTM A29/A29M, 5135 to ASTM A331-95, 5135 to ASTM A519, G51300 to ASTM A1031, G51320 to ASTM A1031, UNS G51300, UNS G51320, UNS G51350, UNS H51300, UNS H51320, UNS H51350 |
| Tradenames: 34 CR 4, AMBO VC 135, ASCOMETAL 32C4, BOHLER KMC, CREUSOT 1F4/5, CREUSOT 1F5/6, FORTUNA TC4, KRUPP 28 CR 4, KRUPP 28 CRS 4, KRUPP 32 CRB 4, KRUPP 34 CRS 4, POMPEY DK 35, SAARSTAHL 34 CR 4, SCHNEIDER 1F 3/4, SCHNEIDER 1F 4/5, STEEL 34 CR 4, SUWEFA TC4, TKS 34CR4, VR-30 |