How do the AISI 8660 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 8660 (UNS G86600) side by side for 2 conditions: Oil Quenched & Tempered at 540°C, Oil Quenched & Tempered at 650°C. All values are taken from the individual AISI 8660 material data sheets linked below.
AISI 8660 Yield, Tensile and Hardness by Condition
| Condition | Yield strength (MPa) | Tensile strength (MPa) | Hardness (HV) | Elongation (%) |
|---|---|---|---|---|
| Oil Quenched & Tempered at 540°C | 1090–1340 | 1180–1440 | 330–410 | 13–21 |
| Oil Quenched & Tempered at 650°C | 855–1050 | 955–1180 | 280–350 | 16–24 |
AISI 8660 Differences Compared with Oil Quenched & Tempered at 540°C
The table below shows how much each condition differs from the oil quenched & tempered at 540°C condition, based on the mid-point of each range. Positive values mean higher strength or hardness.
| Condition | Yield strength | Tensile strength | Hardness | Elongation |
|---|---|---|---|---|
| Oil Quenched & Tempered at 650°C | -22% | -19% | -15% | +18% |
AISI 8660 Strength and Hardness Charts
AISI 8660 Heat Treatment Key Points
The highest tensile strength is reached in the oil quenched & tempered at 540°C condition (1180–1440 MPa). The softest condition is oil quenched & tempered at 650°C (280–350 HV), which is usually preferred for machining and forming. Raising the tempering temperature from 540°C to 650°C lowers hardness from 330–410 HV to 280–350 HV, trading strength for toughness and ductility.
AISI 8660 Material Data Sheets
AISI 8660 Oil Quenched & Tempered at 540°C | AISI 8660 Oil Quenched & Tempered at 650°C | All AISI 8660 conditions
Looking for AISI 8660 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 8660 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.