AISI 4320 Annealed vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 4320 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 4320 (UNS G43200) side by side for 2 conditions: Annealed, Normalized. All values are taken from the individual AISI 4320 material data sheets linked below.

AISI 4320 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
Annealed380–470520–640150–19023–35
Normalized415–515710–875215–26517–25

AISI 4320 Differences Compared with Annealed

The table below shows how much each condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
Normalized+9%+37%+41%-28%

AISI 4320 Strength and Hardness Charts

AISI 4320 Yield strength (MPa)Annealed380–470Normalized415–515
AISI 4320 Tensile strength (MPa)Annealed520–640Normalized710–875
AISI 4320 Hardness (HV)Annealed150–190Normalized215–265

AISI 4320 Heat Treatment Key Points

The highest tensile strength is reached in the normalized condition (710–875 MPa). The softest condition is annealed (150–190 HV), which is usually preferred for machining and forming.

AISI 4320 Material Data Sheets

AISI 4320 Annealed | AISI 4320 Normalized | All AISI 4320 conditions

Looking for AISI 4320 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4320 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment.