AISI 8640 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 8640 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 8640 Oil Quenched & Tempered at 540°C Overview

AISI 8640 tempered 540°C is AISI 8640 low alloy steel (UNS G86400) in the oil quenched & tempered at 540°C condition. This AISI 8640 tempered 540°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 8640 conditions in our AISI 8640 yield, tensile and hardness comparison. Looking for AISI 8640 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 8640 steel parts in-house and inspects them before shipment.

AISI 8640 Oil Quenched & Tempered at 540°C Designation

AISI 8640
ConditionTempered at 540°C & oil quenched
UNS numberG86400
US nameSAE 8740, ASTM 8640, ASTM G86400, ASTM 8740H, ASTM 8740, ASTM 8640H, ASTM 8640, ~SAE 8640, ~SAE 8640
ISO name41 CrNiMoS 2, 41CrNiMoS2, 41CrNiMo2E, ~41CrNiMo2
JIS (Japanese) nameSNCM240

AISI 8640 Oil Quenched & Tempered at 540°C Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 8640 Oil Quenched & Tempered at 540°C Composition detail

C (carbon)0.38–0.43%
Cr (chromium)0.4–0.6%
Fe (iron)96.6–97.8%
Mn (manganese)0.75–1%
Mo (molybdenum)0.15–0.25%
Ni (nickel)0.4–0.7%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 8640 Oil Quenched & Tempered at 540°C Physical properties

Density7.8–7.9g/cm3

AISI 8640 Oil Quenched & Tempered at 540°C Mechanical properties

Young’s modulus201–212GPa
Specific stiffness25.6–27MN.m/kg
Yield strength (elastic limit)925–1140MPa
Tensile strength990–1220MPa
Specific strength118–145kN.m/kg
Elongation12–20% strain
Compressive strength925–1140MPa
Flexural modulus201–212GPa
Flexural strength (modulus of rupture)925–1140MPa
Shear modulus77–83GPa
Bulk modulus155–173GPa
Poisson’s ratio0.285–0.295 
Shape factor23
Hardness – Vickers308–378HV
Elastic stored energy (springs)2090–3120kJ/m3
Fatigue strength at 10^7 cycles425–491MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
370–564MPa

AISI 8640 Oil Quenched & Tempered at 540°C Impact & fracture properties

Fracture toughness37–64MPa.m0.5
Toughness (G)7.03–18.7kJ/m2

AISI 8640 Oil Quenched & Tempered at 540°C Thermal properties

Melting point1430–1510°C
Maximum service temperature500–530°C
Minimum service temperature-63–-38°C
Thermal conductivity36–46W/m.°C
Specific heat capacity460–500J/kg.°C
Thermal expansion coefficient10.5–13µstrain/°C
Thermal shock resistance367–494°C
Thermal distortion resistance2.97–4.08MW/m
Latent heat of fusion265–280kJ/kg

AISI 8640 Oil Quenched & Tempered at 540°C Electrical properties

Electrical resistivity23–35µohm.cm
Electrical conductivity4.93–7.5%IACS
Galvanic potential-0.51–-0.43V

AISI 8640 Oil Quenched & Tempered at 540°C Magnetic properties

Magnetic typeMagnetic

AISI 8640 Oil Quenched & Tempered at 540°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5200m/s
Mechanical loss coefficient (tan delta)3.5e-4–4.4e-4 

AISI 8640 Oil Quenched & Tempered at 540°C Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed14 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Good
Carbon equivalency0.642 – 0.813

AISI 8640 Oil Quenched & Tempered at 540°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 8640 Oil Quenched & Tempered at 540°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 8640 Oil Quenched & Tempered at 540°C Standards with similar compositions

Argentina: IRAM 8640 to IAS
Australia: 8640 to AS 1444
Hungary: NCMo3 to MSZ 61, NCMo3Z to MSZ 6251
International: 41CrNiMo2E to ISO 4954
Italy: 40NiCrMo2 to UNI 7845
Japan: SNCM 240 to JIS G4053
Mexico: 8637 to NMX-B-203-SCFI, 8637 to NMX-B-300, 8637H to NMX-B-268, 8637H to NMX-B-300, 8640 to NMX-B-203-SCFI, 8640 to NMX-B-300, 8640H to NMX-B-268, 8640H to NMX-B-300, 8642 to NMX-B-300, 8642H to NMX-B-268, 8642H to NMX-B-300
Pan America: 8637 to COPANT 334, 8640 to COPANT 334
Poland: 37HGNM to PN-H-84030, 37HGNM to PN-H-84030/04
USA: 8637, 8637 to ASTM A29/A29M, 8637 to ASTM A322-91, 8637 to ASTM A331-95, 8637 to ASTM A519, 8637 to ASTM A752/A752M, 8637 to ASTM A829/A829M, 8637 to SAE J770, 8637H, 8637H to ASTM A304, 8637H to ASTM A331-95, 8637H to SAE J1268, 8640, 8640 to ASTM A29/A29M, 8640 to ASTM A322-91, 8640 to ASTM A331-95, 8640 to ASTM A519, 8640 to ASTM A752/A752M, 8640 to ASTM A829/A829M, 8640 to SAE J404, 8640H, 8640H to ASTM A304, 8640H to ASTM A331-95, 8640H to SAE J1268, 8642, 8642 to ASTM A29/A29M, 8642 to ASTM A322-91, 8642 to ASTM A331-95, 8642 to ASTM A519, 8642 to ASTM A752/A752M, 8642H, 8642H to ASTM A304, 8642H to ASTM A331-95, 8642H to SAE J1268, 94B40, 94B40 to ASTM A519, G86400 to ASTM A1031, G86420 to ASTM A1031, UNS G86370, UNS G86400, UNS G86420, UNS G94401, UNS H86370, UNS H86400, UNS H86420
Tradenames: DF 40 NI CR MO 2, HEVA-DF-120, MONIX 40, VB-40