D6AC Quenched & Tempered Material Data Sheet

D6AC Quenched & Tempered Material Data Sheet

D6AC Quenched & Tempered Overview

D6AC quenched tempered is D6AC low alloy steel (UNS K24728) in the quenched & tempered condition. This D6AC quenched tempered material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for D6AC parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined D6AC steel parts in-house and inspects them before shipment.

D6AC Quenched & Tempered Designation

D6AC
ConditionQuenched & tempered
UNS numberK24728
US nameAMS 6431, ASTM A646 Grade 9, ASTM A579 Grade 23

D6AC Quenched & Tempered Typical uses

General construction, general mechanical engineering, automotive, pressure vessels, pipework

D6AC Quenched & Tempered Composition detail

C (carbon)0.45–0.5%
Cr (chromium)0.9–1.2%
Fe (iron)95.1–96.5%
Mn (manganese)0.6–0.9%
Mo (molybdenum)0.9–1.1%
Ni (nickel)0.4–0.7%
P (phosphorus)0–0.01%
S (sulfur)0–0.01%
Si (silicon)0.15–0.3%
V (vanadium)0.08–0.15%

D6AC Quenched & Tempered Physical properties

Density7.79–7.87g/cm3

D6AC Quenched & Tempered Mechanical properties

Young’s modulus200–210GPa
Specific stiffness25.5–26.9MN.m/kg
Yield strength (elastic limit)1310–1450MPa
Tensile strength1520–1680MPa
Specific strength167–185kN.m/kg
Elongation7–12% strain
Compressive strength1370–1510MPa
Flexural modulus200–210GPa
Flexural strength (modulus of rupture)1310–1450MPa
Shear modulus76–79.9GPa
Bulk modulus185–195GPa
Poisson’s ratio0.32–0.333 
Shape factor17
Hardness – Vickers400–500HV
Hardness – Rockwell C45–47HRC
Elastic stored energy (springs)4180–5110kJ/m3
Fatigue strength at 10^7 cycles683–835MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
656–869MPa

D6AC Quenched & Tempered Impact & fracture properties

Fracture toughness62–95MPa.m0.5
Toughness (G)19.5–42.4kJ/m2

D6AC Quenched & Tempered Thermal properties

Melting point1260–1580°C
Maximum service temperature432–482°C
Minimum service temperature-58–-28°C
Thermal conductivity48–52W/m.°C
Specific heat capacity461–480J/kg.°C
Thermal expansion coefficient12.4–13.1µstrain/°C
Thermal shock resistance496–560°C
Thermal distortion resistance3.74–4.11MW/m
Latent heat of fusion283–326kJ/kg

D6AC Quenched & Tempered Electrical properties

Electrical resistivity15–38µohm.cm
Electrical conductivity4.54–11.5%IACS
Galvanic potential-0.49–-0.41V

D6AC Quenched & Tempered Magnetic properties

Magnetic typeMagnetic

D6AC Quenched & Tempered Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5050–5180m/s
Mechanical loss coefficient (tan delta)4e-4–9e-4 

D6AC Quenched & Tempered Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed9.14 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Good
Carbon equivalency0.953 – 1.19

D6AC Quenched & Tempered Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

D6AC Quenched & Tempered Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

D6AC Quenched & Tempered Notes

D6AC Quenched & Tempered Warning
Some rare heat treatments of certain alloys may produce values for mechanical properties outside the given ranges, e.g. AISI 9255. tempered at 205C

D6AC Quenched & Tempered Standards with similar compositions

USA: 23 to ASTM A579, D6A to SAE J467, Grade 9 to ASTM A646-95, UNS K23725, UNS K24728
Tradenames: CARPENTER D6-AC, D-6 AC, LADISH D6A, LADISH D6AC, LESCALLOY D6AC VAC-ARC, UNITEMP D6C, VASCO D6AC, WESTIG 46 CR MO V 4