AISI 94B30 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 94B30 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 94B30 Oil Quenched & Tempered at 650°C Overview

AISI 94B30 tempered 650°C is AISI 94B30 low alloy steel (UNS G94301) in the oil quenched & tempered at 650°C condition. This AISI 94B30 tempered 650°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 94B30 conditions in our AISI 94B30 yield, tensile and hardness comparison. Looking for AISI 94B30 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 94B30 steel parts in-house and inspects them before shipment.

AISI 94B30 Oil Quenched & Tempered at 650°C Designation

AISI 94B30
ConditionTempered at 650°C & oil quenched
UNS numberG94301

AISI 94B30 Oil Quenched & Tempered at 650°C Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 94B30 Oil Quenched & Tempered at 650°C Composition detail

B (boron)5e-4–0.003%
C (carbon)0.28–0.33%
Cr (chromium)0.3–0.5%
Fe (iron)97–98.1%
Mn (manganese)0.75–1%
Mo (molybdenum)0.08–0.15%
Ni (nickel)0.3–0.6%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 94B30 Oil Quenched & Tempered at 650°C Physical properties

Density7.8–7.9g/cm3

AISI 94B30 Oil Quenched & Tempered at 650°C Mechanical properties

Young’s modulus206–216GPa
Specific stiffness26.2–27.5MN.m/kg
Yield strength (elastic limit)650–795MPa
Tensile strength740–915MPa
Specific strength82.8–101kN.m/kg
Elongation16–26% strain
Compressive strength650–795MPa
Flexural modulus206–216GPa
Flexural strength (modulus of rupture)650–795MPa
Shear modulus79–85GPa
Bulk modulus159–176GPa
Poisson’s ratio0.285–0.295 
Shape factor35
Hardness – Vickers228–283HV
Elastic stored energy (springs)1010–1490kJ/m3
Fatigue strength at 10^7 cycles346–403MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
300–465MPa

AISI 94B30 Oil Quenched & Tempered at 650°C Impact & fracture properties

Fracture toughness47–78MPa.m0.5
Toughness (G)11–27.4kJ/m2

AISI 94B30 Oil Quenched & Tempered at 650°C Thermal properties

Melting point1460–1510°C
Maximum service temperature610–640°C
Minimum service temperature-68–-43°C
Thermal conductivity46–51W/m.°C
Specific heat capacity425–475J/kg.°C
Thermal expansion coefficient11–13µstrain/°C
Thermal shock resistance250–325°C
Thermal distortion resistance3.68–4.46MW/m
Latent heat of fusion265–280kJ/kg

AISI 94B30 Oil Quenched & Tempered at 650°C Electrical properties

Electrical resistivity15–35µohm.cm
Electrical conductivity4.93–11.5%IACS
Galvanic potential-0.51–-0.43V

AISI 94B30 Oil Quenched & Tempered at 650°C Magnetic properties

Magnetic typeMagnetic

AISI 94B30 Oil Quenched & Tempered at 650°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5120–5250m/s
Mechanical loss coefficient (tan delta)4.9e-4–6.1e-4 

AISI 94B30 Oil Quenched & Tempered at 650°C Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed19.5 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Good
Carbon equivalency0.501 – 0.667

AISI 94B30 Oil Quenched & Tempered at 650°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 94B30 Oil Quenched & Tempered at 650°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 94B30 Oil Quenched & Tempered at 650°C Standards with similar compositions

Mexico: 94B30 to NMX-B-203-SCFI, 94B30 to NMX-B-300, 94B30H to NMX-B-268, 94B30H to NMX-B-300
Pan America: 94B30 to COPANT 514
USA: 94B30, 94B30 to ASTM A29/A29M, 94B30 to ASTM A322-91, 94B30 to ASTM A331-95, 94B30 to ASTM A519, 94B30 to ASTM A752/A752M, 94B30 to SAE J770, 94B30H, 94B30H to ASTM A304, 94B30H to ASTM A331-95, 94B30H to SAE J1268, EX 47, EX 48, EX 49, EX 50, UNS G94301, UNS H94301, UNS K13521