AISI 94B30 steel (UNS G94301) is a low alloy steel. This page lists the AISI 94B30 material data sheets for 5 conditions: oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 94B30 Steel
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
Looking for AISI 94B30 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 94B30 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.