AISI 9260 steel (UNS G92600, EN 60Si7) is a low alloy steel. This page lists the AISI 9260 material data sheets for 3 conditions: oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 9260 Steel
Laminated springs, coil springs, torsion bars of heavy section
Looking for AISI 9260 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 9260 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.