AISI 86B45 Low Alloy Steel

AISI 86B45 Low Alloy Steel

AISI 86B45 Steel Overview

AISI 86B45 steel (UNS G86451) is a low alloy steel. This page lists the AISI 86B45 material data sheets for 5 conditions: oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 86B45 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 86B45 Steel Chemical Composition

B (boron)5e-4 – 0.003 %
C (carbon)0.43 – 0.48 %
Cr (chromium)0.4 – 0.6 %
Fe (iron)96.5 – 97.7 %
Mn (manganese)0.75 – 1 %
Mo (molybdenum)0.15 – 0.25 %
Ni (nickel)0.4 – 0.7 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 86B45 Steel Material Data Sheets

AISI 86B45 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 86B45 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 86B45 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 86B45 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 86B45 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 86B45 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 86B45 Tempering Temperature Comparison (205–650°C): Yield, Tensile & Hardness.

AISI 86B45 Steel Parts from Turkey

Looking for AISI 86B45 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 86B45 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.