AISI 4340 Low Alloy Steel

AISI 4340 Low Alloy Steel

AISI 4340 Steel Overview

AISI 4340 steel (UNS G43400) is a low alloy steel. This page lists the AISI 4340 material data sheets for 8 conditions: annealed, normalized, quenched & tempered, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4340 Steel

High tensile applications, general engineering parts, through-hardened gears, connecting rods and bolts, gun barrels

AISI 4340 Steel Chemical Composition

C (carbon)0.38 – 0.43 %
Cr (chromium)0.7 – 0.9 %
Fe (iron)95.2 – 96.3 %
Mn (manganese)0.6 – 0.8 %
Mo (molybdenum)0.2 – 0.3 %
Ni (nickel)1.65 – 2 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.3 %

AISI 4340 Steel Material Data Sheets

AISI 4340 Annealed Material Data Sheet

AISI 4340 Normalized Material Data Sheet

AISI 4340 Quenched & Tempered Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 4340 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 4340 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4340 Annealed vs Normalized vs Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 4340 Steel Parts from Turkey

Looking for AISI 4340 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4340 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.