AISI 4320 Low Alloy Steel

AISI 4320 Low Alloy Steel

AISI 4320 Steel Overview

AISI 4320 steel (UNS G43200) is a low alloy steel. This page lists the AISI 4320 material data sheets for 2 conditions: annealed, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4320 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 4320 Steel Chemical Composition

C (carbon)0.17 – 0.22 %
Cr (chromium)0.4 – 0.6 %
Fe (iron)95.8 – 97 %
Mn (manganese)0.45 – 0.65 %
Mo (molybdenum)0.2 – 0.3 %
Ni (nickel)1.65 – 2 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 4320 Steel Material Data Sheets

AISI 4320 Annealed Material Data Sheet

AISI 4320 Normalized Material Data Sheet

AISI 4320 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4320 Annealed vs Normalized: Yield, Tensile & Hardness Compared.

AISI 4320 Steel Parts from Turkey

Looking for AISI 4320 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4320 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.