AISI 8620 Annealed vs Normalized: Yield, Tensile & Hardness Compared

How do the AISI 8620 heat treatment properties change from one condition to another? This comparison puts the yield strength, tensile strength and hardness of AISI 8620 (UNS G86200, EN 20NiCrMo2-2) side by side for 2 conditions: Annealed, Normalized. All values are taken from the individual AISI 8620 material data sheets linked below.

AISI 8620 Yield, Tensile and Hardness by Condition

ConditionYield strength (MPa)Tensile strength (MPa)Hardness (HV)Elongation (%)
Annealed345–425480–595140–17024–38
Normalized320–400570–700170–21020–32

AISI 8620 Differences Compared with Annealed

The table below shows how much each condition differs from the annealed condition, based on the mid-point of each range. Positive values mean higher strength or hardness.

ConditionYield strengthTensile strengthHardnessElongation
Normalized-6%+18%+23%-16%

AISI 8620 Strength and Hardness Charts

AISI 8620 Yield strength (MPa)Annealed345–425Normalized320–400
AISI 8620 Tensile strength (MPa)Annealed480–595Normalized570–700
AISI 8620 Hardness (HV)Annealed140–170Normalized170–210

AISI 8620 Heat Treatment Key Points

The highest tensile strength is reached in the normalized condition (570–700 MPa). The softest condition is annealed (140–170 HV), which is usually preferred for machining and forming.

AISI 8620 Material Data Sheets

AISI 8620 Annealed | AISI 8620 Normalized | All AISI 8620 conditions