Designation | |
6061, wrought | |
Condition | T62 (Solution heat-treated and artificially aged) |
UNS number | A96061 |
EN name | EN AW-6061 (EN AW-Al Mg1SiCu) |
EN number | 3.3211 |
Aluminum 6061 T62 Mechanical Properties
Young’s modulus | 68 | – | 71.5 | GPa |
Specific stiffness | 25.1 | – | 26.4 | MN.m/kg |
Yield strength (elastic limit) | 241 | – | 266 | MPa |
Tensile strength | 262 | – | 296 | MPa |
Specific strength | 88.8 | – | 98.2 | kN.m/kg |
Elongation | 6 | – | 11 | % strain |
Compressive strength | 234 | – | 259 | MPa |
Flexural modulus | 68 | – | 71.5 | GPa |
Flexural strength (modulus of rupture) | 241 | – | 266 | MPa |
Shear modulus | 26 | – | 27.3 | GPa |
Bulk modulus | 66.9 | – | 70.3 | GPa |
Poisson’s ratio | 0.33 | – | 0.343 | |
Shape factor | 26 | |||
Hardness – Vickers | 67 | – | 108 | HV |
Elastic stored energy (springs) | 416 | – | 509 | kJ/m^3 |
Fatigue strength at 10^7 cycles | 62 | – | 100 | MPa |
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 60.6 | – | 102 | MPa |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey