Base Fe (Iron) : Fe72-80 / Ni12-14 / Mn6-7 / Si2-3
Impurities: C<3, Cu<0.5, Cr<0.2, P<0.08
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 3 | % |
| Cr | (chromium) | 0 | 0.2 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 72.2 | 80 | % |
| Mn | (manganese) | 6 | 7 | % |
| Ni | (nickel) | 12 | 14 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 2 | 3 | % |
Common Uses:
Turbine generator set pressure covers, switchgear insulator flange housings, terminals, and ducts.
| Similar-composition standards with EN GJSA XNiMn13 7 |
|---|
| International: L-NiMn137 to ISO 2892, S-NiMn137 to ISO 2892 |
| UK: EN-GJSA-XniMn13-7 to BS EN 13835, L-NiMn137 to BS 3468 |
| Germany (W.-Nr).: 0.7652 |
| Germany (DIN): GGG-NiMn 13 7 |
| France (AFNOR): S-NM 13 7 |
| Hungary: S-NiMn137 to MSZ ISO 2892 |
| India: AFG Ni 13 Mn 7 to IS 2749, ASG Ni 13 Mn 7 to IS 2749 |
| Japan: FCA-NiMn 13 7 to JIS G5510, FCDA-NiMn 13 7 to JIS G5510 |
| South Korea: GCA-NiMn 13 7 to KS D 4319, GCDA-NiMn 13 7 to KS D 4319 |
| Sweden: 0772-00 to SIS 140772 |