Designation: Type 204-Cu, wrought
UNS number | S20430 |
US name | AISI 204-Cu |
EN name | X9CrMnCuNB17-8-3 |
EN number | 1.4597 |
Country | Equivalent / Similar Grade |
---|---|
USA | S20430 to ASTM A313/A313M, S20430 to ASTM A959, UNS S20430 |
Tradenames: | CARPENTER TYPE 204-CU STAINLESS |