Base Fe (Iron) : Fe51-60 / Ni34-36 / Si4-6 / Cr1.5-2.5 / Mn0.5-1.5
Impurities: C<2, Cu<0.5, P<0.08
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 2 | % |
| Cr | (chromium) | 1.5 | 2.5 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 51.4 | 60 | % |
| Mn | (manganese) | 0.5 | 1.5 | % |
| Ni | (nickel) | 34 | 36 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 4 | 6 | % |
Common Uses:
Parts for gas turbines, such as housings and support rings, as well as turbo-charger housings and exhaust gas manifolds. Die blocks for pressing titanium.
| Similar-composition standards with EN EN GJSA XNiSiCr35 5 2 |
|---|
| USA (ASTM): A439, Type D-5S |
| Germany (DIN): GGG-NiSiCr 35 5 2 |