Base Fe (Iron) : Fe52-62 / Ni28-32 / Si5-6 / Cr4.5-5.5 / Mn0.5-1.5
Impurities: C<2.6, Cu<0.5, P<0.08
Tradename: NI-RESIST TYPE 4
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 2.6 | % |
| Cr | (chromium) | 4.5 | 5.5 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 51.8 | 62 | % |
| Mn | (manganese) | 0.5 | 1.5 | % |
| Ni | (nickel) | 28 | 32 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 5 | 6 | % |
Common Uses:
Compressor cylinders and pressure vessels for use in low temperatures, as well as pump components for air-blast circuit breakers.
| A. Similar-composition standards with EN EN GJSA XNiSiCr30 5 5 |
|---|
| AFNOR NFA32301 SNSC3055 (France) |
| DIN WNr 0.7680 (Germany) |
| DIN 1694 GGG-NiSiCr3055 (Germany) |
| ISO 2892(73) S-NiSiCr3055 (International) |
| BS 3468 S-NiSiCr3055 (United Kingdom) |
| ASTM A439(94) D-4 (USA) |
| B. Similar-composition standards with EN EN GJSA XNiSiCr30 5 5 |
|---|
| International: L-NiSiCr3055 to ISO 2892, S-NiSiCr3055 to ISO 2892 |
| South Korea: GCA-NiSiCr 30 5 5 to KS D 4319, GCDA-NiSiCr 30 5 5 to KS D 4319 |
| UK: EN-GJSA-XNiSiCr30-5-5 to BS EN 13835 |
| USA: UNS F41005 |
| Hungary: S-NiSiCr2055 to MSZ ISO 2892 |
| Japan: FCA-NiSiCr 30 5 5 to JIS G5510, FCDA-NiSiCr 30 5 5 to JIS G5510 |
| India: ASG Ni 30 Si 5 Cr 5 to IS 2749 |