Base Fe (Iron) : Fe56-64 / Ni34-36 / Si1.5-3 / Mn0.5-1.5
Impurities: C<2.4, Cu<0.5, Cr<0.2, P<0.08
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 2.4 | % |
| Cr | (chromium) | 0 | 0.2 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 56.3 | 64 | % |
| Mn | (manganese) | 0.5 | 1.5 | % |
| Ni | (nickel) | 34 | 36 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 1.5 | 3 | % |
Common Uses:
Compressor cylinders that are designed to function at low temperatures, pressure vessels used in air-blast circuit breakers, and components of pumps are some examples of the types of objects that may be made from EN GJSA XNi35 Cast Iron.
| Similar-composition standards with EN GJSA XNi35 |
|---|
| AFNOR NFA32301 SN35 (France) |
| DIN WNr 0.7683 (Germany) |
| DIN 1694 GGG-Ni35 (Germany) |
| ISO 2892(73) S-Ni35 (International) |
| BS 3468 S-Ni35 (United Kingdom) |
| ASTM A439(94) D-5 (USA) |