Base Fe (Iron) : Fe66-76 / Ni21-24 / Mn1.5-2.5 / Si1-3
Impurities: C<3, Cr<0.5, Cu<0.5, P<0.08
| Elements | Min | Max | % |
|---|---|---|---|
| C (carbon) | 0 | 3 | % |
| Cr (chromium) | 0 | 0.5 | % |
| Cu (copper) | 0 | 0.5 | % |
| Fe (iron) | 66.4 | 76.5 | % |
| Mn (manganese) | 1.5 | 2.5 | % |
| Ni (nickel) | 21 | 24 | % |
| P (phosphorus) | 0 | 0.08 | % |
| Si (silicon) | 1 | 3 | % |
Common Uses:
Pump parts, pressure tanks in air-blast circuit breakers, and low- temperature compression cylinders.
| Similar-composition standards with EN GJSA XNi22 |
|---|
| USA: ASTM A439(94) D-2C |
| USA: MIL-C-24707/5(89) D-2C |
| USA: D-2C to ASTM A439-83, UNS F43002 |
| France: AFNOR NFA32301 SN22 |
| Germany: DIN WNr 0.7670 |
| Germany: DIN 1694 GGG-Ni22 |
| International) ISO 2892(73) S-Ni22 |
| International: S-Ni22 to ISO 2892 |
| Japan: FCDA-Ni 22 to JIS G5510 |
| South Korea: GCDA-Ni 22 to KS D 4319 |
| United Kingdom: EN-GJSA-XNi22 to BS EN 13835, S-2C to BS 3468 |
| United Kingdom: BS 3468 S-2C |
| United Kingdom: BS 3468 S-Ni22 |
| Hungary: S-Ni22 to MSZ ISO 2892 |
| India: ASG Ni 22 to IS 2749 |