| Mechanical properties | Values |
|---|---|
| Young’s modulus | * 190 – 210 GPa |
| Specific stiffness | * 24.3 – 27 MN.m/kg |
| Yield strength (elastic limit) | 760 – 930 MPa |
| Tensile strength | 1.03e3 – 1.2e3 MPa |
| Specific strength | * 97.4 – 119 kN.m/kg |
| Elongation | 10 – 20 % strain |
| Compressive strength | * 760 – 930 MPa |
| Flexural modulus | * 190 – 210 GPa |
| Flexural strength (modulus of rupture) | 760 – 930 MPa |
| Shear modulus | * 74 – 84 GPa |
| Bulk modulus | * 134 – 156 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 28 |
| Hardness – Vickers | * 350 – 420 HV |
| Hardness – Rockwell B | * 109 – 113 HRB |
| Hardness – Rockwell C | * 35 – 43 HRC |
| Hardness – Brinell | * 327 – 400 HB |
| Elastic stored energy (springs) | * 238 – 292 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 436 – 487 MPa |
| Fatigue strength model (stress range) | * 391 – 544 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |