| Mechanical properties | Values |
|---|---|
| Young’s modulus | 193 – 201 GPa |
| Specific stiffness | * 24.7 – 25.9 MN.m/kg |
| Yield strength (elastic limit) | 515 – 760 MPa |
| Tensile strength | 860 – 1.03e3 MPa |
| Specific strength | * 66 – 97.5 kN.m/kg |
| Elongation | 20 – 40 % strain |
| Compressive strength | * 515 – 760 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | 515 – 760 MPa |
| Shear modulus | 75 – 80 GPa |
| Bulk modulus | 136 – 149 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 37 |
| Hardness – Vickers | * 252 – 280 HV |
| Hardness – Rockwell B | * 100 – 103 HRB |
| Hardness – Rockwell C | 23 – 27 HRC |
| Hardness – Brinell | * 240 – 266 HB |
| Elastic stored energy (springs) | 194 – 307 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 385 – 437 MPa |
| Fatigue strength model (stress range) | * 334 – 504 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |