Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding
| Mechanical properties | Values |
|---|---|
| Young’s modulus | 193 – 201 GPa |
| Specific stiffness | * 24.7 – 25.9 MN.m/kg |
| Yield strength (elastic limit) | 760 – 930 MPa |
| Tensile strength | 1.03e3 – 1.21e3 MPa |
| Specific strength | * 97.4 – 119 kN.m/kg |
| Elongation | 10 – 20 % strain |
| Compressive strength | * 760 – 930 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | 760 – 930 MPa |
| Shear modulus | 75 – 80 GPa |
| Bulk modulus | 136 – 149 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 28 |
| Hardness – Vickers | * 302 – 334 HV |
| Hardness – Rockwell B | * 105 – 108 HRB |
| Hardness – Rockwell C | 30 – 34 HRC |
| Hardness – Brinell | * 285 – 317 HB |
| Elastic stored energy (springs) | 2.19e3 – 2.38e3 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 436 – 490 MPa |
| Fatigue strength model (stress range) | * 389 – 550 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |