Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding |Turkiye
Composition detail | % |
---|---|
C (carbon) | 0 – 0.15 % |
Cr (chromium) | 15.5 – 17.5 % |
Cu (copper) | 2 – 4 % |
Fe (iron) | * 64.5 – 74.4 % |
Mn (manganese) | 6.5 – 9 % |
N (nitrogen) | 0.05 – 0.25 % |
Ni (nickel) | 1.5 – 3.5 % |
P (phosphorus) | 0 – 0.06 % |
S (sulfur) | 0 – 0.03 % |
Si (silicon) | 0 – 1 % |
*Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |