| Mechanical properties | Values |
|---|---|
| Young’s modulus | 193 – 201 GPa |
| Specific stiffness | * 24.7 – 25.9 MN.m/kg |
| Yield strength (elastic limit) | 930 – 965 MPa |
| Tensile strength | 1.21e3 – 1.28e3 MPa |
| Specific strength | * 119 – 124 kN.m/kg |
| Elongation | 7 – 10 % strain |
| Compressive strength | * 930 – 965 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | 930 – 965 MPa |
| Shear modulus | 75 – 80 GPa |
| Bulk modulus | 136 – 149 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 24 |
| Hardness – Vickers | * 344 – 382 HV |
| Hardness – Rockwell B | * 109 – 111 HRB |
| Hardness – Rockwell C | 35 – 39 HRC |
| Hardness – Brinell | * 326 – 362 HB |
| Elastic stored energy (springs) | 2.35e3 – 2.55e3 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 489 – 509 MPa |
| Fatigue strength model (stress range) | * 469 – 531 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |