POM-H vs POM-C

POM-H vs POM-C 1. GENERAL INFORMATION (POM-H vs POM-C) Item POM-H (Homopolymer) POM-C (Copolymer) Designation Polyoxymethylene, acetal (homopolymer) Polyoxymethylene, acetal (copolymer) Tradenames Accucomp, Altech, Ashlene, Astatal, Bergaform, Bestpom, Celcon, Cheng, Cress-Atal, Delrin, Duracon, Duratuf, Edgetek, Hostaform, Hostaform Xap², Isoform, Iupital, Kebaform, Kepital, Kocetal, Latan, Lucel, Next Regrind, Pier, Poliform, Polyform, Ramtal, Schulaform, Sindustris, Stat-Loy, Tarnoform, … Continue reading POM-H vs POM-C