NIMONIC PE16 (bar) Material Data Sheet
Nickel-Fe-Cr alloy, NIMONIC PE16, bar NIMONIC PE16 Designation INCO Inc. Proprietary Alloy: “NIMONIC PE16” NIMONIC PE16 Tradenames NIMONIC PE16 Special Metals Corp. (USA) NIMONIC PE16 Typical uses Aerospace NIMONIC PE16 Composition detail Al (aluminum) 1 % Cr (chromium) 16.5 % Fe (iron) 34.4 % Mo (molybdenum) 3.2 … Continue reading NIMONIC PE16 (bar) Material Data Sheet