INCOLOY 800 Material Data Sheet (Spring Temper, Wire)

Nickel-Fe-Cr alloy, INCOLOY 800, spring temper, wire INCOLOY 800 Designation (spring temper, wire) Unified Numbering System (USA): N08800 Condition Spring temper UNS number N08800 US name ASTM Grade N08800; AMS 5766, 5871 EN name X 10 NiCrAlTi 32 20 EN number 1.4876 ISO name ISO 9723, 9724, 9725, 6207, 6208 INCOLOY 800 Tradenames (spring temper, … Continue reading INCOLOY 800 Material Data Sheet (Spring Temper, Wire)