FERRITIC, MARTENSITIC & PRECIPITATION HARDENING STAINLESS STEEL COMPARISON TABLE
Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding | Engineering | Turkiye | Turkey EURONORM/DIN W. Nr. AISI UNS AFNOR BRAND X 6 Cr 13 1.4000 410 S S 41008 Z 8 C 12 … Continue reading FERRITIC, MARTENSITIC & PRECIPITATION HARDENING STAINLESS STEEL COMPARISON TABLE