EN GJN HV600 (XCr18) Mechanical Properties, former BS 3C, Cast iron, white, high-chromium alloy

EN GJN HV600 (XCr18) Mechanical Properties,former BS 3C Min Max Young’s modulus 165 220 GPa Specific stiffness 21.1 28.3 MN.m/kg Yield strength (elastic limit) *300 450 MPa Tensile strength 300 450 MPa Specific strength *38.4 57.8 kN.m/kg Elongation *1 2 % strain Compressive strength *500 900 MPa Flexural modulus *165 220 GPa Flexural strength (modulus … Continue reading EN GJN HV600 (XCr18) Mechanical Properties, former BS 3C, Cast iron, white, high-chromium alloy