EN GJN HV600 (XCr11) Chemical Composition, former BS 3G, Cast iron, white, high-chromium alloy

Compositional summary Fe73-87 / Cr11-14 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1) Material family: Metal (ferrous) Base material: Fe (Iron) Elements Min Max % C (carbon)   1.8 – 3.6 % Cr (chromium)   11 – 14 % Cu (copper)   0 – 2 % Fe (iron)   72.8 – 87.1 … Continue reading EN GJN HV600 (XCr11) Chemical Composition, former BS 3G, Cast iron, white, high-chromium alloy