EN GJN HV600 Chemical Composition, former BS 2D, Cast iron, white, Ni-Cr alloy

Compositional summary Fe76-83 / Cr8-10 / Ni4.5-6.5 / C2.5-3.5 / Si1.5-2.5 / Mn0.2-0.8 (impurities: Mo<0.5, S<0.15, P<0.1) Material family: Metal (ferrous) Base material: Fe (Iron) Elements Min Max % C (carbon) 2.5 3.5 % Cr (chromium) 8 10 % Fe (iron) 76.1 83.3 % Mn (manganese) 0.2 0.8 % Mo (molybdenum) 0 0.5 % Ni … Continue reading EN GJN HV600 Chemical Composition, former BS 2D, Cast iron, white, Ni-Cr alloy