EN 10088-3 Standard Guide Stainless steels-Part 3: Technical delivery conditions for semifinished products, bars, rods, wire, sections and bright products of corrosion resistant steels for general purposes PRODUCT FORMS & SURFACE FINISHES HOT FORMED PRODUCTS Symbol Full Description Surface Finish Typical Use Tolerance Range 1U Hot formed, NOT heat treated, NOT descaled Covered with scale (spot ground if necessary). Not free of surface imperfections. For further hot forming – 1C Hot formed, heat treated, NOT descaled … Continue reading EN 10088-3 Standard Guide