Aluminum, EN AC-48000, chill cast, T6 Material Data Sheet

Aluminum, EN AC-48000, chill cast, T6 Aluminum, EN AC-48000, chill cast, T6 Designation EN AC-48000 (DIN EN 1706) Condition T6 (Solution heat-treated and artificially aged) EN number EN AC-48000 / EN AC-AlSi12CuNiMg Aluminum, EN AC-48000, chill cast, T6 Typical uses High strength alloy for the automotive industry: space frames, wheels, axle and differential housings, pump, … Continue reading Aluminum, EN AC-48000, chill cast, T6 Material Data Sheet