Aluminum 5456 (annealed) Material Data Sheet Aluminum 5456 Designation 5456, wrought Condition O (Annealed) UNS number A95456 EN name EN AW-5456 (EN AW-Al Mg5Mn1(A)) Aluminum 5456 Typical uses Armor plate, high strength welded structures, storage tanks, pressure vessels, marine service Aluminum 5456 Composition detail Al (aluminum) 92 – 94.8 % Cr (chromium) 0.05 – 0.2 … Continue reading Aluminum 5456 Material Data Sheet