Aluminum 5454 Material Data Sheet

Aluminum 5454 (annealed) Material Data Sheet Aluminum 5454 Designation 5454, wrought Condition O (Annealed) UNS number A95454 EN name EN AW-5454 (EN AW-Al Mg3Mn) EN number 3.3537 Aluminum 5454 Typical uses Welded structures, pressure vessels, tube for marine service Aluminum 5454 Composition detail Al (aluminum) 94.4 – 97 % Cr (chromium) 0.05 – 0.2 % … Continue reading Aluminum 5454 Material Data Sheet