Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding Mechanical properties Values Young’s modulus  * 193 – 201 GPa Specific stiffness  * 24.5 – 25.6 MN.m/kg Yield strength (elastic limit)  304 – 336 MPa Tensile strength  650 … Continue reading AISI 201LN Stainless steel (Low nickel work hardenable), austenitic, Annealed | Mechanical Properties