AISI 201 Stainless steel (Low nickel work hardenable), austenitic, 1/2 hard | Mechanical Properties

Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding Mechanical properties Values Young’s modulus  193 – 201 GPa Specific stiffness  * 24.7 – 25.9 MN.m/kg Yield strength (elastic limit)  760 – 930 MPa Tensile strength  1.03e3 – … Continue reading AISI 201 Stainless steel (Low nickel work hardenable), austenitic, 1/2 hard | Mechanical Properties