EN GJSA XNiSiCr35 5 2 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe51-60 / Ni34-36 / Si4-6 / Cr1.5-2.5 / Mn0.5-1.5 Impurities: C<2, Cu<0.5, P<0.08 Elements Symbol Elements Name Min Max % C (carbon) 0 2 % Cr (chromium) 1.5 2.5 % Cu (copper) 0 0.5 % Fe (iron) 51.4 60 % Mn (manganese) 0.5 1.5 % Ni (nickel) 34 36 % P (phosphorus) 0 … Continue reading EN GJSA XNiSiCr35 5 2 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY